Skip to content
FiftyOhm
Esc
  • Air-core coilSingle-layer air-core solenoid inductance from Nagaoka's exact coefficient, compared with Wheeler's formula. Solve for the number of turns for a target inductance.Components & magnetics
  • Attenuator PadsResistor values for Pi, T, bridged-T and minimum-loss L-pad attenuators, with unequal impedances, power dissipation per resistor and E24/E96 rounding.Couplers, dividers & attenuators
  • CoaxCoax Z0, capacitance and inductance per length, velocity factor, loss, exact TE11 cutoff and breakdown voltage. Solve for D, d or εr from Z0.Transmission lines
  • CPW / GCPWCoplanar waveguide and grounded CPW impedance, effective permittivity, dispersion, delay and loss by conformal mapping. Solve for centre width or gap.Transmission lines
  • dBm ↔ W ↔ VConvert RF power between dBm, dBW, watts, Vrms, Vpeak, Vpp, dBµV and dBmV for any system impedance. Instant, accurate, with formulas.Fundamentals & conversions
  • Differential pairEdge-coupled microstrip and stripline differential impedance, Z0 even/odd, common-mode impedance, coupling and delay. Solve for spacing or width from Zdiff.Transmission lines
  • Filter OrderMinimum filter order to meet a passband/stopband attenuation mask for Butterworth, Chebyshev and elliptic responses, with the attenuation actually achieved.Filters
  • Free-space path lossFree-space path loss from the Friis equation, received power with antenna gains, and a far-field check. Solve for distance or frequency.Propagation & link budget
  • L / Pi / T MatchingDesign lumped L, Pi and T matching networks between complex source and load impedances. Both L solutions, loaded-Q Pi/T, component values and bandwidth.Matching & Smith chart
  • LC Filter DesignerDesign lumped LC ladder filters: Butterworth, Chebyshev or Bessel; low-pass, high-pass, band-pass, band-stop to order 10, with exact insertion loss and group delay.Filters
  • MicrostripMicrostrip Z0, effective permittivity, dispersion, delay and loss. Solve for trace width from target impedance. Hammerstad–Jensen + Kirschning–Jansen models.Transmission lines

Skin Depth Calculator

Skin depth and surface resistance for copper, silver, gold, aluminium, nickel, brass, tin, stainless or a custom metal, plus the frequency where δ equals thickness.

5 cited sources17 reference checksRuns in your browser

Inputs

Used for the frequency at which δ equals the thickness and for the t/δ ratio.

Results

Skin depth(δ)
2.0898
Surface resistance(Rₛ)
8.2502
Frequency where δ = t(f_δ=t)
3.5651
Thickness / skin depth(t/δ)
16.75
Conductivity used(σ)
58
Permeability used(μr)
1
  • Values assume bulk, smooth metal at about 20 °C. Conductivity falls roughly 0.4 %/°C for copper, and surface roughness raises the effective loss.

Formulas

δ=1πfμ0μrσ\delta = \frac{1}{\sqrt{\pi f \mu_0 \mu_r \sigma}}Rs=1σδ=πfμ0μrσR_s = \frac{1}{\sigma\delta} = \sqrt{\frac{\pi f \mu_0 \mu_r}{\sigma}}fδ=t=1πμ0μrσt2f_{\delta = t} = \frac{1}{\pi \mu_0 \mu_r \sigma t^2}

What this calculator does

At DC, current spreads evenly over a conductor's cross-section. At high frequency, the changing magnetic field inside the metal induces eddy currents that oppose the current in the interior, and the current crowds towards the surface. The current density falls off exponentially with depth, and the skin depth δ is the depth at which it has dropped to 1/e1/e (37 %) of its surface value:

δ=1πfμ0μrσ\delta = \frac{1}{\sqrt{\pi f \mu_0 \mu_r \sigma}}

Skin depth sets the RF resistance of every conductor. If the metal is several skin depths thick, it behaves like a sheet of thickness δ, and its resistance per square is the surface resistance

Rs=1σδ=πfμ0μrσ.R_s = \frac{1}{\sigma\delta} = \sqrt{\frac{\pi f \mu_0 \mu_r}{\sigma}}.

RsR_s goes straight into the conductor-loss equations of transmission lines, cavities and antennas. Because it grows as f\sqrt{f}, conductor loss in dB per metre also grows as f\sqrt{f}, until dielectric loss takes over.

The calculator also reports the frequency at which δ equals a given thickness,

fδ=t=1πμ0μrσt2,f_{\delta=t} = \frac{1}{\pi\mu_0\mu_r\sigma t^2},

and the ratio t/δt/\delta. Above this frequency the conductor no longer behaves like a DC conductor. Below it, the thickness, not the skin effect, limits the resistance.

Materials

The presets use room-temperature (about 20 °C) bulk values.

Materialσ (MS/m)Source
Copper, annealed58.0IEC 60028 annealed-copper standard (100 % IACS)
Silver63.0CRC Handbook, ρ = 1.587 µΩ·cm at 293 K
Gold45.2CRC Handbook, ρ = 2.214 µΩ·cm
Aluminium37.7CRC Handbook, ρ = 2.650 µΩ·cm
Nickel14.4CRC Handbook, ρ = 6.93 µΩ·cm (μr entered separately)
Brass, cartridge (C26000)16.228 % IACS (typical alloy value)
Tin8.70ρ = 11.5 µΩ·cm
Stainless steel 3041.39ρ = 72 µΩ·cm (typical alloy value)

Pure copper is slightly better than the IACS standard: CRC gives 59.6 MS/m. The 58.0 MS/m standard is the usual design value for commercial annealed copper and PCB foil. Choose Custom to enter any conductivity and permeability.

Nickel is the exception. It is ferromagnetic, and its permeability depends strongly on frequency: it can be a few hundred at low frequency and falls towards 1 above its ferromagnetic resonance, in the low-GHz range. It also depends on the plating process and on the field strength. When you choose nickel, the calculator shows the μr input. Enter a value that applies at your frequency, and it warns you if you leave μr at 1. This matters for ENIG finishes, where a few microns of nickel sit under a thin gold layer and can add noticeable loss below a few GHz.

How to use solve-for

  • Solve Frequency for Skin depth to find where δ reaches a target. For example, enter 1 µm to see where a 1 µm plating starts to carry most of the current.
  • Frequency where δ = t is already a direct output. Solving Conductor thickness for it gives the thickness that equals one skin depth at a frequency.
  • Solve Conductor thickness for t/δ = 3 to find the thickness that is three skin depths at your frequency. In a conductor that thick, 95 % of the current (1−e−31 - e^{-3}) flows within the conductor.

Worked example

Copper at 1 GHz:

  • skin depth δ = 2.090 µm;
  • surface resistance RsR_s = 8.250 mΩ per square;
  • 1 oz foil (t=35 μt = 35\,\mum) is t/δt/\delta = 16.75 skin depths thick;
  • δ equals 35 µm at 3.565 MHz.

At 1 GHz, the other presets give δ = 2.005 µm for silver, 2.368 µm for gold, 2.591 µm for aluminium, 5.397 µm for tin and 13.50 µm for 304 stainless.

As a cross-check against the literature: at 10 GHz, with σ = 5.8×10⁷ S/m, textbooks quote δ = 6.6×10⁻⁵ cm (0.66 µm), and this calculator gives 0.6609 µm.

Accuracy and validity

The formula is exact for a flat, smooth, homogeneous conductor much thicker than δ, with a frequency-independent conductivity. It also holds for curved conductors whose radius of curvature is much larger than δ. Its limitations are in the inputs and in a few physical effects:

EffectImpact
TemperatureCopper's σ falls about 0.39 %/°C, so δ grows about 0.2 %/°C. At 85 °C, RsR_s is about 12 % higher than at 20 °C
Surface roughnessA real foil with roughness comparable to δ has 1.2–2× (and more) the smooth-surface loss
Thin conductors (t≲3δt \lesssim 3\delta)The current also flows on the back surface; the resistance does not follow RsR_s
Alloys and platingsConductivity varies with composition and process, often ±10 % or more
Above ~1 THz or at cryogenic temperatureThe anomalous skin effect and carrier relaxation break the classical model

Practical notes

  • Platings. A finish thinner than about one skin depth is largely transparent: the current flows mostly in the metal underneath. Thick silver plating on brass gives silver-like loss above a few hundred MHz.
  • Thicker copper doesn't help at RF. Above a few tens of MHz, extra copper weight barely reduces conductor loss, because the current lives within a few microns of the surface. On a microstrip, most of it flows on the underside of the trace, next to the dielectric, where the foil is roughest.
  • Litz wire works only at low frequency. Stranded insulated wire reduces skin and proximity losses only while each strand is thinner than about δ, which in practice limits it to below a few MHz.
  • Shielding. The absorption loss of a shield is 8.69 dB per skin depth of thickness, which is why thin copper shields work well at RF but poorly at power-line frequencies, where δ in copper is about 8.5 mm at 60 Hz.

References

  1. S. Ramo, J. R. Whinnery and T. Van Duzer, Fields and Waves in Communication Electronics, 3rd ed., Wiley, 1994, ch. 3 (penetration of fields into good conductors, internal impedance).
  2. D. M. Pozar, Microwave Engineering, 4th ed., Wiley, 2012, ch. 1 (plane waves in a good conductor, surface resistance).
  3. CRC Handbook of Chemistry and Physics, CRC Press, “Electrical Resistivity of Pure Metals” (293 K: Ag 1.587, Cu 1.678, Au 2.214, Al 2.650, Ni 6.93; Sn 11.5 ×10⁻⁸ Ω·m).
  4. IEC 60028, International Standard of Resistance for Copper, 1925 (annealed copper standard, 58.0 MS/m at 20 °C).
  5. ASM Handbook, Vol. 2 (cartridge brass C26000, 28 % IACS) and Vol. 1 (AISI 304 stainless, 72 µΩ·cm), ASM International.

This calculator's results are checked against 17 independent reference values in automated tests on every change. How we check accuracy.